The disc harrow absorbs the advantages of similar foreign advanced products, and is designed according to the standard. The outer spherical inner square hole sealed rolling bearing, the disc harrow has the advantages of reasonable structure, strong and durable, convenient transportation, small turning radius, easy adjustment, maintenance and so on. The harrow is the main core component of the disc harrow, which is an important factor related to the level of the disc harrow. Let's take a look at it in detail:
1. The hardness is uneven. During cladding, the disc harrow may cause uneven hardness due to the uneven thickness of the cladding layer. Areas where the cladding layer is too hard are usually caused by ten carburizing, that is, the operator inserts the flame core of the oxygen-acetylene flame into the molten cladding layer or the length ratio of the inner flame core is ten 3:1. Areas of lower hardness in the cladding are usually the result of the incorporation of ten base metals into the cladding.
2. Cracks. Low preheating temperature before cladding, poor control of cladding process (temperature drop too fast) and rapid cooling after cladding. It is easy to cause cracks in the cladding layer. Therefore, preheating and post-cooling before cladding is an important feature of oxy-acetylene flame cladding of nickel-based cemented carbide. In addition, the operation diagram of the disc harrow, the deposition on the unannealed quenched parts is also prone to cracks. If the crack of the deposited layer has propagated into the base metal, the crack needs to be completely removed with a grinding wheel (or removed by other machining methods). Then preheat, weld, and cool slowly according to the specified process. If the crack does not propagate to the base metal, the part can be re-heated and penetrated to eliminate the crack.